|| Parameter || ITMs || ETMs || PRM || SRM || FM (4x) ||
|| HR Transmission 1064 nm || 0.014|| 10 ppm || || || <0.01 ||
|| HR Transmission 532 nm || < 1000 ppm|| 0.10 || || || ||
|| AR Reflection 1064 nm || 1000 ppm|| < 100 ppm || || || <0.01 ||
|| AR Reflection 532 nm || <0.01|| < 1000 ppm || || || ||
|| ROC || inf|| 40 m? || || || inf||
|| Wedge angle || 1 deg || 1 deg || || || ||
|| Parameter || ITMs || ETMs || PRM || SRM || FM (4x) ||
|| HR Transmission 1064 nm || 0.014 * || 10 ppm ||0.055 +/-0.003 ||0.10 +/- 0.005 || <0.01 ||
|| HR Transmission 532 nm || < 1000 ppm || 0.10 ||n/a ||n/a ||n.r. ||
|| AR Reflection 1064 nm || < 1000 ppm || < 100 ppm ||< 300 ppm ||< 300 ppm || <0.01 ||
|| AR Reflection 532 nm || <0.01 || < 1000 ppm ||n/a ||n/a || ||
|| ROC || Flat (>5 km) || 57.5 m? ||115.5 96.3 +50/-0 (96**) || 142 117.1+50/-20 (116.3**) || inf ||
|| Wedge angle || 1 deg (+/- 0.2 deg) || 1 deg ||1 deg ||1 deg ||1 deg ||


[[BR]][[BR]]*''T_ITMnom = 0.014 +/- 0.002. All 3 ITMs in the same coating run to match the T, i.e. T_ITMY - T_ITMX < 0.0003. Tolerance in T_ITMnom is larger.''** Based on ETM and ITM ROC, assuming inf. thin optics.
----
 . Draft zip file of specs in .doc format: attachment:40mCOC-080723.zip (need to change the ext to .doc)
 . Also in [javascript:void(0);/*1254859239474*/ [PDF]]

----
 . Specs of the folding mirrors for the recycling cavities

|| Name || PR1 || PR2 || SR1 || SR2 ||
|| Size ||2"dia. X 3/8" thick ||2"dia. X 3/8" thick ||2"dia. X 3/8" thick ||2"dia. X 3/8" thick ||
|| Incident angle || 2.5 deg || 36.5 deg || 39.9 deg || 17.1 deg ||
|| HR Transmission 1064 nm || 500ppm || < 100 ppm || < 100ppm || < 100ppm ||
|| AR Reflection 1064 nm || < 0.25% || < 0.25% || < 0.25% || < 0.25% ||
|| ROC || Flat || Flat || Flat || Flat ||
|| Wedge angle || 1 deg || 1 deg ||1 deg ||1 deg ||
||Qty. || 2 || 2 || 2 || 2 ||


----
 . [[Upgrade 08/Optics/RCParams|Considerations on the parameters of PRC/SRC]]

'''Communication between ATF and Coastline'''

{{{
From: Gene Lapp
Sent: Tuesday, July 28, 2009 4:00 PM
To: Ramin Lalezari Cc: Vern Korn; John Tardif (E-mail)
Subject: Power Recycling Mirrors / Signal Recycling Mirrors

Ramin,

I've run across another small problem with the Power Recycling & Signal Recycling Mirrors. The wedge angle is called out as 2° 30' ± 5'. The parts are measuring between 2° 40' and 2° 44' (all ± 0.5'). We have traced this problem to an error in our wedge tool, which is nominally at 2° 40'.

All the mirrors have been measured except for one Signal Recycling Mirror (currently on the polishing machine). I expect that it will be in the same condition. The measurements are as follows:

PRMU01 2° 40'
PRMU02 2° 42'
PRMU03 2° 43'
PRMU04 2° 40' (extra)

SRMU01 -
SRMU02 2° 41'
SRMU03 2° 41'
SRMU04 2° 44' (extra)
}}}

Coatings and Optics

This is a work in progress area for what optic and coatings we need.

Parameter

ITMs

ETMs

PRM

SRM

FM (4x)

HR Transmission 1064 nm

0.014 *

10 ppm

0.055 +/-0.003

0.10 +/- 0.005

<0.01

HR Transmission 532 nm

< 1000 ppm

0.10

n/a

n/a

n.r.

AR Reflection 1064 nm

< 1000 ppm

< 100 ppm

< 300 ppm

< 300 ppm

<0.01

AR Reflection 532 nm

<0.01

< 1000 ppm

n/a

n/a

ROC

Flat (>5 km)

57.5 m?

115.5 96.3 +50/-0 (96**)

142 117.1+50/-20 (116.3**)

inf

Wedge angle

1 deg (+/- 0.2 deg)

1 deg

1 deg

1 deg

1 deg

BRBR*T_ITMnom = 0.014 +/- 0.002. All 3 ITMs in the same coating run to match the T, i.e. T_ITMY - T_ITMX < 0.0003. Tolerance in T_ITMnom is larger.** Based on ETM and ITM ROC, assuming inf. thin optics.


  • Draft zip file of specs in .doc format: attachment:40mCOC-080723.zip (need to change the ext to .doc)
  • Also in [javascript:void(0);/*1254859239474*/ [PDF]]


  • Specs of the folding mirrors for the recycling cavities

Name

PR1

PR2

SR1

SR2

Size

2"dia. X 3/8" thick

2"dia. X 3/8" thick

2"dia. X 3/8" thick

2"dia. X 3/8" thick

Incident angle

2.5 deg

36.5 deg

39.9 deg

17.1 deg

HR Transmission 1064 nm

500ppm

< 100 ppm

< 100ppm

< 100ppm

AR Reflection 1064 nm

< 0.25%

< 0.25%

< 0.25%

< 0.25%

ROC

Flat

Flat

Flat

Flat

Wedge angle

1 deg

1 deg

1 deg

1 deg

Qty.

2

2

2

2


Communication between ATF and Coastline

From: Gene Lapp
Sent: Tuesday, July 28, 2009 4:00 PM
To: Ramin Lalezari Cc: Vern Korn; John Tardif (E-mail)
Subject: Power Recycling Mirrors / Signal Recycling Mirrors

Ramin,

I've run across another small problem with the Power Recycling & Signal Recycling Mirrors.  The wedge angle is called out as 2° 30' ± 5'.  The parts are measuring between 2° 40' and 2° 44' (all ± 0.5').  We have traced this problem to an error in our wedge tool, which is nominally at 2° 40'.

All the mirrors have been measured except for one Signal Recycling Mirror (currently on the polishing machine).  I expect that it will be in the same condition.  The measurements are as follows:

PRMU01    2° 40'
PRMU02    2° 42'
PRMU03    2° 43'
PRMU04    2° 40'  (extra)

SRMU01    -
SRMU02    2° 41'
SRMU03    2° 41'
SRMU04    2° 44'  (extra)